STEEL IMPEX INDIA · ALLOY STEEL · HARDEN · TEMPER · ANNEAL
Heat treatment chart for C40E, 42CrMo4, 34CrNiMo6 and 100Cr6
Choose the alloy grade and check the producer’s heat-treatment guidance for annealing, normalising, hardening or tempering. Match the stock section and required delivery condition with the certificate and order. Confirm the actual furnace cycle, quench and mechanical requirements with the mill or a qualified heat-treatment provider for the part.
Read the mill’s published heat-treatment guidance alongside the exact steel grade, condition and treatment step. Each row links to the original source so you can check the material and context. For a delivered bar, use the inspection documents to establish the treatment and test results for that particular heat.
Each row gives the steelmaker’s guidance for the named grade in degrees Celsius. The mill sheet also identifies related designations. Use the ordered grade, section size, required properties and the heat treater’s procedure to select the cycle.
How the names relate
The mill sheets list related designations alongside the steel used for each treatment schedule. For enquiries using an older British or SAE designation, check the specification on the material certificate. See the EN19 and EN24 grade references.
| Related designation | Grade in the mill sheet | Soft anneal | Normalise | Harden and quench | Temper | Notes | Source |
|---|---|---|---|---|---|---|---|
| EN8 / BS 080M40 | C40E / 1.1186 | 690, air | 850-890, air | 830, water; or 870, oil/polymer | 550-660, air | Stress relief: 50 °C below tempering temperature. Hot forming: 1100 down to 850 °C. | Lucefin, C40E technical card, rev. 2024, pp. 1-2 |
| BS 709M40 | 42CrMo4 / 1.7225 | 680-720, furnace | 850-880, air | 820-860, oil or water | 540-680, air | Soft-annealed (+A) condition: 241 HB maximum. The mill also lists SAE 4140H and 4140RH. | Saarstahl, 42CrMo4 / 42CrMoS4, p. 1 |
| BS 817M40 | 34CrNiMo6 / 1.6582 | 650-680, furnace | 850-880, air | 830-860, oil | 540-660, air | Hot forging or rolling: 1100 down to 850 °C. The mill also lists SAE 4337 and 4340. | Saarstahl, 34CrNiMo6, p. 1 |
| BS 535A99 | 100Cr6 / 1.3505 | 780-800, furnace | 870-900, air | 830-870, oil; or 800-830, water | 150-180 | Hardened and tempered surface hardness: approximately 62 HRC. | Saarstahl, 100Cr6, p. 1 |
Sources: Mill heat-treatment data: Lucefin C40E and Saarstahl 42CrMo4, 34CrNiMo6 and 100Cr6 · Source register
- Unit
- °C
- Last verified
Read each temperature with the cooling medium shown in its cell. Section size, hold time and acceptance criteria follow the ordered material and process specification.
Download the reference PDF
Grade reference: heat treatment, stainless finishes and PREN. The PDF holds the same tables as the pages, generated from the same data, with the verification date in the footer.
Sources and last verified
- Lucefin, C40E technical card, rev. 2024, pp. 1-2
- Saarstahl, 42CrMo4 / 42CrMoS4, p. 1
- Saarstahl, 34CrNiMo6, p. 1
- Saarstahl, 100Cr6, p. 1
Last verified: . Verify against the applicable standard and edition named in your purchase order.
Common questions
How does Saarstahl heat treat 42CrMo4?
Its sheet specifies hardening at 820-860 °C with oil or water cooling, followed by tempering at 540-680 °C with air cooling.
How does Saarstahl temper 34CrNiMo6?
Its sheet gives 540-660 °C with air cooling after hardening at 830-860 °C with oil cooling.
What surface hardness does Saarstahl report for 100Cr6?
The sheet gives approximately 62 HRC at the surface after hardening and tempering.
Which condition should I match before using a data row?
Match the grade designation, product form and treatment condition to the cited mill sheet. An entry for another condition may describe a different material response.
Can this chart establish how a delivered bar was treated?
Ask for the heat-treatment condition and relevant test results on the bar’s inspection documents. A mill’s published reference row does not identify the treatment history of an individual bar.