STEEL IMPEX INDIA · PREN · PITTING · STAINLESS AND NICKEL ALLOYS
PREN calculator (pitting resistance equivalent number)
Calculate the pitting resistance equivalent number with the chosen formula and the chromium, molybdenum and nitrogen values reported on your certificate. Use tungsten only for a formula that includes it. Compare values on the same basis, and confirm corrosion suitability separately for the actual product and service environment.
Estimate the pitting resistance equivalent number from the alloy composition and the formula selected in the calculator. Use reported percentages for an identified heat when available. Keep the formula and composition together when comparing results, and assess the actual service conditions separately before choosing a material.
PREN ranks stainless steels and nickel alloys by their resistance to pitting in chloride solutions. Enter the chromium, molybdenum and nitrogen of a heat (from the mill certificate), or load an available grade preset with its cited composition source. PREN is a ranking index, not a prediction of behaviour in a particular medium, temperature or crevice.
Calculator
Enter your values and press Calculate. The result appears here.
Formula
PREN = %Cr + 3.3 × %Mo + 16 × %N (mass %)Tungsten-bearing grades: PREN = %Cr + 3.3 × (%Mo + 0.5 × %W) + 16 × %NSome duplex specifications use 30 × %N instead of 16 × %N; the specification you buy to decides.
Worked example
A duplex heat with 22.0 % Cr, 3.0 % Mo and 0.17 % N: 22.0 + 3.3 × 3.0 + 16 × 0.17 = 34.6 (with 30 N: 37.0).
| Grade | Calculated envelope and heat requirement | Composition table used |
|---|---|---|
| SS 317L | 27.9 to 34.8 | ATI 317L plate analysis limits, mass % |
| Duplex 2304 | 22.5 to 29.7 | Jindal J-2304 flat-product analysis limits, mass % |
| NITRONIC 50 / XM-19 | 28.7 to 39.8 | Electralloy published product analysis ranges and maxima, mass % |
Sources: Steel Impex India grade dataset (each row cites its own source) · Source register
- Formula
PREN = Cr + 3.3 Mo + 16 N, using mass %. A maximum-only limit has a lower mathematical bound of zero- Unit
- PREN to 1 decimal
- Last verified
Each envelope combines independent chemistry limits. Only sources with publication review and upper limits for Cr, Mo and N are included. Use the measured heat analysis for other grades.
Sources and last verified
- Pitting resistance equivalent number (cites ASM Handbook Vol. 13B, Corrosion: Materials, 2005, p. 58): PREN = Cr + 3.3 Mo + 16 N; variants with 30 N and 3.3 (Mo + 0.5 W)
- Grade composition limits: Steel Impex India grade dataset and source register
Last verified: . Verify against the applicable standard and edition named in your purchase order.
Common questions
What is a good PREN for seawater?
PREN only ranks alloys. Seawater suitability also depends on temperature, crevices, flow and fabrication, so take the alloy choice from the equipment specification or a corrosion engineer, not from PREN alone.
Why does a grade have a PREN range?
The calculated endpoints combine the individual minimum or maximum values. A product specification can also impose a minimum on the combined result. Check that minimum using the chemistry from the heat certificate.
Which nitrogen factor should I use, 16 or 30?
The common form uses 16. Some duplex specifications define PREN with 30; use the formula written in the specification you buy to.
Should I enter a grade range or a heat analysis?
For one heat, enter the reported alloy percentages from its certificate. A grade preset represents its stated composition basis and can differ from the result for that heat.
Can I compare results calculated with different formulas?
Recalculate both compositions with the same formula before comparing their numbers. Record the formula alongside the composition so someone else can repeat the comparison.
Published by Steel Impex India · Technical reference policy