Aluminium 7475 equivalents, chemistry & properties.

Aluminium 7475 is a aluminium (wrought) used for mostly used for aircraft fuselage and wing skins needing high toughness. Below are its equivalent designations in nine standards, chemical composition, mechanical properties and density.

Aluminium 7475 equivalent grades

USA (ASTM / AISI / SAE)
7475
UNS
A97475
Europe (EN)
EN AW-7475 (AlZn5.5MgCu(A))
China (GB)
7475

Key data

Family
Aluminium (wrought)
Density
2.81 g/cm³
Typical mechanical
T7351: TS about 490 MPa; high fracture toughness
Typical uses
Mostly used for aircraft fuselage and wing skins needing high toughness
Weight
Calculate weight in Aluminium 7475

Aluminium 7475 chemical composition (weight %)

SiFeCuMnMgCrZnTi
≤0.10≤0.121.2–1.9≤0.061.9–2.60.18–0.255.2–6.2≤0.06

Grades similar to Aluminium 7475

Frequently asked questions

What is the equivalent of Aluminium 7475?

Aluminium 7475 equivalents: USA (ASTM / AISI / SAE) 7475; UNS A97475; Europe (EN) EN AW-7475 (AlZn5.5MgCu(A)); China (GB) 7475. Equivalents are close but not always identical; check the standard on your order.

What is the chemical composition of Aluminium 7475?

Aluminium 7475: Si ≤0.10, Fe ≤0.12, Cu 1.2–1.9, Mn ≤0.06, Mg 1.9–2.6, Cr 0.18–0.25, Zn 5.2–6.2, Ti ≤0.06 (weight %).

What is the density of Aluminium 7475?

About 2.81 g/cm³ (2,810 kg/m³), the value used for weight calculations.